Note that they are coming from all over the plating on the connector... not
necessarily just from the solder joints... So tin finishes are also possible
sources for tin whiskers. Whew... scares me worse than Freddy Kruger at the
door for trick-or-treat ever could...
Happy Halloween...
BTW I have pasted the link on a new page on my website... I'm going to run a
lead free blog of interesting things I find out on there for anyone to use
as a quick reference to lead free issues.
The web page is http://www.pcbwizards.com/leadfree.htm
cheers
Bill Brooks - KG6VVP
PCB Design Engineer, C.I.D.+, C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
Datron World Communications, Inc.
_______________________________________
San Diego Chapter of the IPC Designers Council
Communications Officer, Web Manager
http://dcchapters.ipc.org/SanDiego/
http://pcbwizards.com
-----Original Message-----
From: Franklin Asbell [mailto:[log in to unmask]]
Sent: Tuesday, October 11, 2005 11:05 AM
To: [log in to unmask]
Subject: Re: [TN] RoHS Process Compliant boards
(chuckle) Wow, impressive growth...Looks more like spider webs than
whiskers...
Franklin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bloomquist, Ken
Sent: Tuesday, October 11, 2005 12:53 PM
To: [log in to unmask]
Subject: Re: [TN] RoHS Process Compliant boards
You have to make sure you have the entire link (both lines) in order to
get to the web page. The only way I was able to get it to work was copy
and paste the first line into Internet Explorer, don't open it and copy
and paste the second line to the end of the first line. Hit Enter and it
should work.
KennyB
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Franklin Asbell
Sent: Tuesday, October 11, 2005 10:48 AM
To: [log in to unmask]
Subject: Re: [TN] RoHS Process Compliant boards
I'm having trouble locating the horror pictures...which article exactly?
Franklin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brooks,Bill
Sent: Tuesday, October 11, 2005 12:11 PM
To: [log in to unmask]
Subject: Re: [TN] RoHS Process Compliant boards
Have you seen some of the horror pictures in the recent article from
advanced packaging? Gives me the chills!
http://ap.pennnet.com/Articles/Article_Display.cfm?Section=ARTCL&ARTICLE
_ID=
233627&VERSION_NUM=2&p=95
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|