MIL-P-18177 is a pre-curser to MIL-P-13949. In the early years of epoxy
systems, they did not have flame resistance, which was found to be an
issue quickly. When the DOD began to develop a specification for a
flame resistance system, they opted to create a new spec - MIL-P-13949
rather that revise the old spec as several manufactures still were
producing to 18177 and could not produce a new epoxy at that time.
Eventually (1992) this spec was cancelled without replacement.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice: 802.257.4571.21 Fax: 802.257.0011
http://www.vtcircuits.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Parsons
Sent: Friday, October 14, 2005 10:59 AM
To: [log in to unmask]
Subject: [TN] MIL-P-18177
Good morning all,
I have a customer spec'ing a PCB from laminate meeting MIL-P-18177/GEE.
I
can't seem to find a copy of the MIL-P-18177 spec but an internet search
turns up reference to this spec and FR-4/G10 materials. None of my
material
spec sheets make reference however. Can anyone shed some light on this
requirement.
TIA
John Parsons
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|