Looks like the finger to the left of the arrow is thinking about peeling
also. Not that I am an expert but my recommendation would be strip and
replate all of them. Do it now and not have to worry or deal with it on
a customer return in a couple months or sooner.
The bigger question would be what caused this to occur. You get all the
way thru Conformal Coat then this happens. Not a happy ending...
Randy Bock Sr.
Quality Manager
Pitney Bowes
AddressRight Printers
(email) [log in to unmask]
Newtown Building 2
203 270-4931 Ext
8-426-4931 In
203 270-4982 Fax
Steve Gregory <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
10/28/2005 11:37 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] Gold Plating Peeling...
Well, I just got back from "Sin City", and as they say; "no rest for the
wicked".
I really wasn't that wicked, but I was confronted with a new problem this
morning.
We just built some assemblies and conformal coated them, but when they
were
being
de-masked, the gold plating on the fingers started peeling up! Check out:
http://www.stevezeva.homestead.com/files/Peeling_Plating.jpg
http://www.stevezeva.homestead.com/files/Peeling_Plating_2.jpg
I have a couple of questions:
Can I repair this?
If I repair this, should all fingers be stripped and repaired?
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc. It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|