TECHNET Archives

October 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Gabriela Bogdan <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 28 Oct 2005 16:12:20 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ingemar Hernefjord <[log in to unmask]>
Subject:
From:
Ingemar Hernefjord <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
<00ba01c5dba7$1d55c9b0$10851bac@gabideaf82jrvb>
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (130 lines)
Gaby, think you need a real good repair equipment to begin with. We
started with simple ones, but realized that handling and repairing up to
SBGA 2,500 need precision and repeatability and no human errors. We have
two machines, like the below. There are lots of such machines on the
market.

http://www.ape.com/sniper_wide.html

http://www.ape.com/images/Brochure%20Sniper%20III%20Low%20Res.pdf

http://www.focalspot.com/rd500.html

We repair and replace CSP and BGA daily, just works fine. To replace a
BGA with these machines takes just a few minutes. We never do just
reflow on suspect boards, but go directly to replacement. Too risky
relying on reflow only. 

Inge



-----Ursprungligt meddelande-----
Från: Gabriela Bogdan [mailto:[log in to unmask]] 
Skickat: den 28 oktober 2005 12:05
Till: Ingemar Hernefjord; 'TechNet E-Mail Forum'
Ämne: Re: [TN] BGA failure and assembly repair

Thanks, Inge, I will try to do it.
I was thinking also about the design of the boards, like stress factors 
after soldering.I can not eliminate those- we are just assembling a wide

variety of boards and we don't always know what happes after assembly.
I was thinking also about the residual stresses in the BGA-like
warping.Each 
failure has its own footprint, which I recognize. The question is, what 
others are doing usually when they have to repair a BGA site- what is
their 
experience in reliability and cost?
IPC speaks only about replacing.Is there someone who is doing additional

reflow on the old component as a repair method? Is it considered
reliable?
Gaby
----- Original Message ----- 
From: "Ingemar Hernefjord" <[log in to unmask]>
To: "'TechNet E-Mail Forum'" <[log in to unmask]>; "'Gabriela Bogdan'" 
<[log in to unmask]>
Sent: Friday, October 28, 2005 12:41 PM
Subject: SV: [TN] BGA failure and assembly repair


> Gaby,
> If the BGAs are OK, and your is process OK, then I can't see better
> solution than search for a better board supplier.
>
> You'd better send some pics on the cross sections. You told us nothing
> about the failure freqency per position, per board, batch dependency,
> and variations by time. To change supplier is of course a question of
> what the failures cost you.
>
> Inge
>
> -----Ursprungligt meddelande-----
> Från: TechNet [mailto:[log in to unmask]] För Gabriela Bogdan
> Skickat: den 28 oktober 2005 09:37
> Till: [log in to unmask]
> Ämne: [TN] BGA failure and assembly repair
>
> Dear Technetters!
>
> We sometimes receive failed boards from the field with failures on
BGA's
> for  repair.
> Supposing there is no problem with the BGA as a component, supposing
> that the X-ray test (feinfocus tiger) does not reveal any problems in
> the solder joints (with exception to cracks which are very hard to
> detect), what procedure would you suggest?
> We are concerned with the following:
> Reliability
> Cost: the assemblies are still our responsability
> We are considering:
> Scrap
> Repair by reflow and electrical test
> Repair by installing a new component and electrical test- this
includes
> the possibility of visual inspection of the area under the failed
> component and finding more out about the failure mechanism)
> Lately we have performed several destructive tests in order to  see
the
> nature of the failures which could not be repaired by reflow, and
found:
> through hole cracks or corrosion in plugged holes
> pad lifting and conductor cracks
> solder joint cracks
> All these were not detected by X-ray.
> Could you suggest the best procedure?
>
> Gaby
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
> ext.2815
> -----------------------------------------------------
>
>
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2