Hi Werner,
I was told by some that this delam is not a rejectable criteria per
some industry standards. While I have not sought out these standards to see
for myself, based upon what you are saying, perhaps my second assessment may
be what we have to live with. Thanks for the feedback, Werner.
Best regards,
Leo
Director of Applications Engineering
ASAT, Inc.
3755 Capital of Texas Highway, Suite 100
Austin, Texas 78704
ph 512-383-4593
fx 512-383-1590
[log in to unmask]
www.asat.com
The information contained in this electronic message is CUSTOMER/SUPPLIER
PRIVILEGED AND CONFIDENTIAL INFORMATION intended only for the use of the
individual or entity named above. If the reader of this message is not the
intended recipient, you are hereby notified that any dissemination,
distribution and copying of this communication is strictly prohibited. If
you have received this communication in error, please immediately notify the
sender by electronic mail. Thank you.
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Wednesday, October 19, 2005 6:41 PM
To: [log in to unmask]; [log in to unmask]
Subject: Re: [TN] Delamination at Thermal Via area?
Hi Leo,
I am afraid you might be stuck with (2); for 2 reasons.
(1) I do not see 'resin recession' in either via barrel walls [IPC documents
except after soldering processes] ir burried (thermal) vias as a reliability
risk--where is the risk?;
(2) no matter what you do, the adhesion will likely never be enough; you
could fill the filling resin more to get its CTE closer to Cu.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|