Sona:
I do not recommend your "plating" the lead out of your Tin/Lead bath, it is too uncontrolled.
(And actually, it would, theoretically, take you forever to get to true "no-lead"..it would just keep getting less and less.)
I do recommend you start over, using the fluoborate electrolyte system, rather than the sulfate, or methane sulfonate system.
Sorry to have been unclear in my recommendation.
I think the Fluoborate electrolyte is THE way to go, but if you go there, do it suddenly, not gradually.
And always remember, free advice is often not worth what you paid for it...
Rudy Sedlak
---------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Yahoo! Music Unlimited - Access over 1 million songs. Try it free.
|
|
|