TECHNET Archives

October 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"morand, garry" <[log in to unmask]>
Date:
Fri, 7 Oct 2005 13:55:57 -0400
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "morand, garry" <[log in to unmask]>
Parts/Attachments:
text/plain (122 lines)
Franklin-

Check into Allied High Tech's MetPrep 3.  It's an auto grinder/polisher
that's able to polish 1, 2, or 3 mounts individually depending on your need.
You can get the info off the web.  Used may be a problem though.  Struers
and Buehler, as well as a few other metallographic supply companies do/may
offer similar products.

Still I would recommend grinding 8 and 10 mil dhs PTHs manually, then
polishing automatically if you want.  Hitting the center shouldn't be a prob
for this large a hole size!  Clear mounting media is paramount for this.

anything smaller is getting into difficulty.

At first I thought you wanted Buehler's minimet which is a single mount
automatic grinder/polisher, very light force, and not needed for PCBs.

Best regards,
Garry Morand
EMC Corp.
Hopkinton MA

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Franklin Asbell
Sent: Friday, October 07, 2005 8:47 AM
To: [log in to unmask]
Subject: Re: [TN] Microsection

(chuckle) No, that thought hadn't hit me... So you're suggesting I continue
till I can hit a 6 mil hole with my shaky hands? Well okay, I'll continue.

Franklin

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair K. Hogg
Sent: Friday, October 07, 2005 7:33 AM
To: [log in to unmask]
Subject: Re: [TN] Microsection

Franklin,

Have you considered that you may be a pioneer in what you are trying to do
and that no one here can offer any advice cause nobody has tried it before?

Blair

>>> [log in to unmask] 10/07/05 07:02AM >>>
(chuckle)

Yes, can you believe it... got no response at all, now Steve, they jumped
all over his request, I'm thinking it has to do with his website and he
allowing people to post pictures, and so people want to keep him
happy...(laughing as people wonder how serious I am) luckily I'm past that
point where I would take it personal, but years ago....hmmm, well anyway.

What I'm looking for is a device to grind/polishing a single mount (3 pc
board coupons in a single puck) by hand.

In days past I could do a somewhat decent job, with todays smaller holes,
even down past 10 to 8 and even 6 I find it difficult to hit the center of
the hole +/- 10%.

Beuhler makes what they call the PC-Met jr, selling cost $2500 for the kit
which is crazy as they sell the complete kit for 6 mounts at $4500.

So I'm looking for a used unit, or one from another source (not even sure
who else might make one, perhaps Struers)

So that's my need today...any suggestions would be wonderful.

Franklin


*******************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they
are addressed. If you have received this email in error please notify
the system manager.

This footnote also confirms that this email message has been swept
for the presence of computer viruses.

www.hubbell.com - Hubbell Incorporated

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2