Morning Everybody!
As some of you might have read in my past posts, I don't have much
capability (read: none) for microsectioning PCB's in-house, other than
a Dremel tool and a desire to try and see things.
Things look like they will possibly be changing in the future as far as
our microsectiong needs...we will need to have at least a basic capability
in-house to do a decent microsection. One of the things besides PCB
sections
that we will be looking at, is to be able to verify void-free underfill.
I'd like to ask those of you that do microsections all the time for a
favor. If
you had to set-up a basic capability from scratch, what would be the
minimum
things that you like to have. I can fumble around and eventually get
everything
I need, but I thought; "Why re-invent the wheel?" So I thought I would ask
you all...
Just off the top of my head, these are some of the basic things of what I
think I
should have:
1. Diamond saw
2. Series of grinding/polishing wheels
3. Potting molds
4. Potting materials
5. High magnification microscope
6. ?
If there are things that you would add to the list, please add them for me.
If there
are certain vendors of the things on the list that you feel are better than
others,
go ahead and list them as well. If you feel that you should respond
off-line on
those items, do that as well.
I'm not trying to set-up a full blown failure analysis lab, just something
that will give
us the capability to spot some of the obvious problems from a microsection.
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc. It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|