can you check using sem/edx see if it is TiO2 or some others? It should be
TiO2 I believe...someone may replaced by others..
White Pigment Discovery Date
White Lead 4th century before Christ
Zinc Oxide middle of 18th century
Lithopone middle of 19th century
Anatase TiO2 1919
Rutile TiO2 1939
jk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Franklin Asbell
Sent: Thursday, September 08, 2005 12:38 PM
To: [log in to unmask]
Subject: [TN] Pink symbol ink...
We got a call from a customer expressing an interesting issue.
They ran product through their wave solder and the symbolization went from
white to pink.
I've never heard of this color change appearing, anyone out there have an
idea?
The symbol is Enthone 50-100R - white, the wave solder info I have is Type R
flux with a peak temperature of 215 C.
Appreciate any input, thanks.
Franklin
pI
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|