TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Wolfgang E. Erat" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Wolfgang E. Erat
Date:
Tue, 6 Sep 2005 21:59:23 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (56 lines)
Hi, sounds to me like the old jet pumice scrubbing, and yes, by some stretch
you can picture this a sandblasting. Not sure how widely used this is these
days but it sure does a good job.

Wolfgang

----- Original Message -----
From: "Ivanoe Pedruzzi" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, September 06, 2005 9:34 AM
Subject: [TN] Sand blasting pcb after copper etching


> Dear Technetters,
>
> I'm not familiar with the process of making pcb and I would like to
> have your comments on something I was told from a pcb maker
> representative.
>
> "...in order to ensure a well insulation between traces, we do
> sandblasting (very little and tiny) pcb's after etching.
> this is to remove the bonding material that remains on the board after
> removing the copper. This is the only way to achieve a very good SIR
> result."
>
> Is this a normal procedure, was he correct in his claim?
>
>
> Thanks,
> Ivanoe Pedruzzi
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2