Hi All,
Pls inform if you have good experience with such applications for Aluminium
pins to be soldered on PCBs.
The electric parameters are as follow:
Nickel: EMF = -0.15volt and Anodic index = 30
Aluminium: EMF = -0.60volt and Anodic index = 75
Tin: EMF = -0.50volt and Anodic index = 65
Electroless Nickel thickness 15 micron, Tin plated thickness 8 micron.
Reuven ROKAH
e mail: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------