Michael - we have the luxury of owning an Auger as well as running high
volumes of ENIG through our plant. We purchased an Auger when we were
running 20,000 panels/week of electroless Pd as this tool is exactly
what
you need for surface analysis. It will be of no use for determining the
presence of black nickel as the definition of "black nickel" has yet to
be
accepted. Can it determine the amount of phos at the interface - yes,
can it
determine the amount of phos in the bulk - absolutely, both indicators
of
the quality of how the bath was controlled/maintained by the board
supplier,
and something that is cited as indicative of the presence of black
nickel.
Can it pick up other contaminants like Cu, etc in the deposit - yes. It
will
pick up Ni as you scan the Au surface. It can pick up residues
associated
with solder mask or dry film residues. You may wish also to expand it to
use
XPS and have them identify the relative oxidation states of the elements
found - can be more informative than just identifying the presence of
something - great for showing excessive rinsing/hold times post Ni
plating
that passivates the surface impacts solderability.
If you wish to contact me off line with specifics.
Regards
Gerard O'Brien
Photocircuits Corporation
Co-Chairman 4-14 plating committee.
-----Original Message-----
From: Arbour, Michel [mailto:[log in to unmask]]
Sent: Tuesday, September 20, 2005 4:12 PM
To: [log in to unmask]
Subject: [TN] ENIG contaminant : Auger analysis recommended ?
Hi
We will be sending non solderable PCB for analysis. Goal is to detect
black
nickel, black pad, soldermask contamination before plating or other
contaminant. Is Auger analysis with ion sputtering (SAM) an effective
method
to determine the contaminants. Is this method proven and accepted in the
PCB
industry for this task ?
Michel Arbour
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|