TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard" <[log in to unmask]>
Date:
Thu, 29 Sep 2005 12:08:52 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Phillip Bavaro <[log in to unmask]>
Subject:
From:
Phillip Bavaro <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (106 lines)
I second the AirVac DRS-24 recommendation.  I have used one for about five years and have complete confidence in it for post assembly installation of BGA down to .5 mm pitches because it has good process controls.

Programming it takes a little getting used to but what custom software doesn't.

If money was not tight, I would actually prefer to buy their ONYX system as it has a lot more capability and is fire wire controlled.



"Stadem, Richard" <[log in to unmask]> wrote:
I recommend that you check out the AirVac DRS24 or DRS26. These are
excellent rework machines for the general range of 10 mm sqare to about
50 mm square package sizes on pwbs that are up to .125" thick on boards
up to about 14" x 14" or so. They provide the best process control on
the market.
Anything larger or more demanding you will probably need a Summit (also
an excellent machine), or a larger AirVac.
For smaller flip-chip and up to a medium BGA size and medium board size,
Metcal/Ok Ind. machines are very good. They have precise airflow
control, which is needed for very small, low mass flip chips or small
CSPs. They also have excellent vision alignment systems.
Stay far away from infrared systems. They do not heat the assembly
and/or the board evenly in the surrounding area, and the ability to soak
the entire assembly is non-existent. Get a machine with a large
bottomside preheat capacity, 1000 watts or better. It is critical to
pre-heat the entire assembly evenly to prevent damage to the pwb during
the rework cycle.
Infrared is useless when working with silicon flipchips or CSPs. They
are essentially glass mirrors and the infrared machines work poorly or
not at all with them.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair K. Hogg
Sent: Thursday, September 29, 2005 8:30 AM
To: [log in to unmask]
Subject: [TN] BGA Rework Station Recommendations

I've proposed to management that since we will need a BGA rework station
if/when we begin using BGAs, and since our current old pick and place
machines aren't up to the task, and that since our initial usage at
first will be low volume (5 to 10 per month) assemblies, that we look
into procuring the rework station and use it for the initial placement
of the BGAs after reflow (or maybe even carefully carry the placed
assemblies to the rework station, place the BGA, the carefully carry
back to the oven for reflow). Naturally, I got assigned the task of
researching equipment and making the recommendation.

Do you have any recommendations on what equipment would be best suited
for this, or what you have and what you like and don't like about it?

You can send replies offline if you would like.

Thanks,

Blair Hogg
QA Manager
GAI-Tronics Corporation

*******************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they are
addressed. If you have received this email in error please notify the
system manager.

This footnote also confirms that this email message has been swept for
the presence of computer viruses.

www.hubbell.com - Hubbell Incorporated

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------
Yahoo! for Good

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
 Click here to donate to the Hurricane Katrina relief effort.

ATOM RSS1 RSS2