TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 26 Sep 2005 06:43:03 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ofer Cohen <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Ofer Cohen <[log in to unmask]>
Parts/Attachments:
text/plain (115 lines)
Bill,
I agree with George, and can add only that while calling colleges about experience with surface finish listen carefully to those who were experience with some types.
 
Ofer Cohen
Seabridge - a Siemens company

________________________________

From: TechNet on behalf of Wenger, George M.
Sent: Sun 9/25/2005 6:51 PM
To: [log in to unmask]
Subject: Re: [TN] lead free PCB Replacement Coatings



Bill,

Those who like ENIG (Electroless Nickel under Immersion Gold) are going
to tell you it's great and there should be no problems with using it
with SAC305 and VOC-Free flux.  Those who use IAg (Immersion Silver) are
also going to tell you it's great and there should be no problems with
using it with SAC305 and VOC-Free flux.  I'm one of those who use IAg
and believe that it is a good surface finish for standard SnPb assembly
or Pb-Free assembly.  If I were to tell you about the potential problems
with using ENIG there would be those out there who would tell you that
there aren't any problems. I would suggest that you not listen to any
PCB fabricator who can only provide with one or the other and I also
wouldn't listen to any supplier who sells surface finish chemistry.  Ask
as many PCB users as you can and find out what their experience has been
with different surface finishes and then make an informed decision.  As
I indicated, IAg is the surface finish we prefer.  But as I indicated
I'm only one user.

Regards,
George
George M. Wenger, Andrew Corporation
Reliability / FMA Engineer
Base Station & Subsystems Group
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 [log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Sunday, September 25, 2005 12:32 PM
To: [log in to unmask]
Subject: Re: [TN] lead free PCB Replacement Coatings

To All:  Have have read many articles regarding what folks are
recommending
as replacement coating for HASL.  What are folks experiences  with
Electroless
Gold and also Electroless Silver?  Is one substantially  cheaper than
the
other?  Are there benefits of one over the other?
Will either cause any potential problems when using SAC 305 and a VOC
free
flux?

Thanks in advance for help with these issues!!!!!!

Bill Black
Q.A. Manager
Medco
631-667-9699
[log in to unmask] (mailto:[log in to unmask])

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information. 
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2