I also agree with Mr. Wenger.
I have tons of experience with both Immersion Silver and ENIG. I have
also used immersion tin, HASL, and OSP finishes extensively.
I have never had any trouble with immersion silver. I have had trouble
with the others, especially ENIG.
No matter what anyone says, there are tons of instances where
reliability issues came up with ENIG. These are well documented, as are
the root causes.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ofer Cohen
Sent: Sunday, September 25, 2005 11:43 PM
To: [log in to unmask]
Subject: Re: [TN] lead free PCB Replacement Coatings
Bill,
I agree with George, and can add only that while calling colleges about
experience with surface finish listen carefully to those who were
experience with some types.
Ofer Cohen
Seabridge - a Siemens company
________________________________
From: TechNet on behalf of Wenger, George M.
Sent: Sun 9/25/2005 6:51 PM
To: [log in to unmask]
Subject: Re: [TN] lead free PCB Replacement Coatings
Bill,
Those who like ENIG (Electroless Nickel under Immersion Gold) are going
to tell you it's great and there should be no problems with using it
with SAC305 and VOC-Free flux. Those who use IAg (Immersion Silver) are
also going to tell you it's great and there should be no problems with
using it with SAC305 and VOC-Free flux. I'm one of those who use IAg
and believe that it is a good surface finish for standard SnPb assembly
or Pb-Free assembly. If I were to tell you about the potential problems
with using ENIG there would be those out there who would tell you that
there aren't any problems. I would suggest that you not listen to any
PCB fabricator who can only provide with one or the other and I also
wouldn't listen to any supplier who sells surface finish chemistry. Ask
as many PCB users as you can and find out what their experience has been
with different surface finishes and then make an informed decision. As
I indicated, IAg is the surface finish we prefer. But as I indicated
I'm only one user.
Regards,
George
George M. Wenger, Andrew Corporation
Reliability / FMA Engineer
Base Station & Subsystems Group
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Sunday, September 25, 2005 12:32 PM
To: [log in to unmask]
Subject: Re: [TN] lead free PCB Replacement Coatings
To All: Have have read many articles regarding what folks are
recommending as replacement coating for HASL. What are folks
experiences with Electroless Gold and also Electroless Silver? Is one
substantially cheaper than the other? Are there benefits of one over
the other?
Will either cause any potential problems when using SAC 305 and a VOC
free flux?
Thanks in advance for help with these issues!!!!!!
Bill Black
Q.A. Manager
Medco
631-667-9699
[log in to unmask] (mailto:[log in to unmask])
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
------------------------------------------------------------------------
------------------------
This message is for the designated recipient only and may contain
privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender immediately
and delete the original. Any unauthorized use of this email is
prohibited.
------------------------------------------------------------------------
------------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|