TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 9 Sep 2005 11:17:15 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Tempea, Ioan" <[log in to unmask]>
Parts/Attachments:
text/plain (36 lines)
Yep,

good considerations on the gloves, thank you.

But what about my original dilemma, wear gloves on assemblies that will be washed or not? Or, why wearing gloves when you cook, since you are boiling the ingredients anyways?

And yeah, hockey is good, but football (real football, that you guys call soccer) is better. Sorry, but I had to mention it, since I started the whole thing...

Thanks again,
Ioan

> -----Original Message-----
> From: Tempea, Ioan 
> Sent: Thursday, September 08, 2005 2:38 PM
> To:   [log in to unmask]
> Subject:      Clean before cleaning
> 
> Technos,
> 
> the question is whether to wear or not to wear gloves on assemblies that will be washed. I am fully aware of the solderability problems that can occur without gloves, so let's stick strictly to the post-wash contamination.
> 
> And in the same key, Doug was talking about not using white gloves that have chlorines due to bleaching. Which are the gloves to wear?
> 
> Thank you,
> Ioan

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2