I've used with marginal success, a Tig welder and coat hanger wire, touch-up
afterwards made this method cost prohibitive so I purchased IPC 7711, there
are much better methods suggested in that manual...I recommend it. Not sure
if it would meet Telcordia though...
Franklin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gus Morvillo
Sent: Friday, September 30, 2005 4:00 PM
To: [log in to unmask]
Subject: [TN] Wires / Straps
Hello,
Could anyone suggest a method or technology used to permanently add a
wire / strap to a board. I'm trying to find out if there is an
acceptable method, such that it would pass IPC or Telcordia standards.
Thanks
/g
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|