Clearly you don't want to create additional problems when doing rework. A
process would need to be developed that would allow the rework to occur
without interfering with any previous components on the product.
On boards already reworked I would not touch again if the solder meets IPC
610 (at whatever class you are inspecting).
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mary Jane Chism
Sent: Thursday, September 29, 2005 2:21 PM
To: [log in to unmask]
Subject: [TN] Solder Protrusions
We are experiencing icicles (solder protrusions) as the results of
rework being performed on a flatpak. The process is hot air removal of
the flat pak and hand soldering for replacement. In the process of hand
soldering, the operators are touching some of the surface mount
capacitors around the flat pak causing solder protrusions off of the
solder fillet of the capacitors.
In IPC-A-610, it states as long as the solder protrusions do not violate
height requirement and electrical clearance, they would be acceptable.
However, I feel the objective of performing rework is that you only
perform the operation of soldering without putting any thermal stress on
the rest of the components.
I realize this is hard for anyone to actually answer this, but my
question is, if you can answer this, would you:
1. Re-address your rework process and also get rid of the icicles?
2. Re-address your rework process but let the icicles go?
3. Don't do the rework?
4. Get different rework operators to perform the rework?
Your comments will be very much appreciated.
Thanks.
Mary Jane Chism
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|