Hi Richard,
Tin-lead plating is appied to a PWB as an etch resist. However, it is
co-plated tin and lead, not solder, and thus does not provide a protection for the
underlying copper. Therefore it needs to be heated--fused, to make solder out of
it, but in this process forms a miniscus, not a very flat. Thus, it needs to
be hot-air-solder-levelled, which means excess liquid solder is simply blown
off the surface creating a much flatter surface.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|