If you have a good solder connection the bumps will not affect the
function - in fact you likely have better adhesion of the devices with
more surface area.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice: 802.257.4571.21 Fax: 802.257.0011
http://www.vtcircuits.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, September 14, 2005 10:57 AM
To: [log in to unmask]
Subject: Re: [TN] [OT]...sorta RE: [TN] raised vias...I did a "Okie"
cross-section
You're right Dewey. Geeze, always correcting me...
I shoulda' said; I did a "Okie-dokie" Okie cross-section, huh?
Speaking of which, I went back it at again this morning for a bit.
Went deeper and deeper, and the width of the hole in the via did
not change much, which tells me that I was pretty much in the center
of the via....and as was commented earlier, they did a heck of a job
plating the walls of the vias...that's some thick walls of copper.
I got to a point where I could start seeing the back wall of the hole,
because some of the resin was coming out of the hole from the gentle
scraping I was doing with the exacto knife, and yes, now I believe that
is
pre-preg resin coming up through the blind via hole during lamination to
the thick copper core.
You can see my latest image at:
http://www.stevezeva.homestead.com/files/Cross_Section.jpg
This is a image that was taken from our SmartScope Flash system
at somewhere around 200 magnification.
Now comes the big question, are the bumps a reliability issue? I did see
some open/insufficient solder defects in the first build of these
boards.
We
touched things up for the most part, before I knew what was causing the
defects.
I can compensate for the insufficient solder problems probably by
getting
a
thicker stencil, so should I worry about these bumps?
-Steve-
|---------+------------------------------->
| | "Whittaker, Dewey |
| | (AZ75)" |
| | <Dewey.Whittaker@HON|
| | EYWELL.COM> |
| | Sent by: TechNet |
| | <[log in to unmask]> |
| | |
| | |
| | 09/14/2005 08:38 AM |
| | Please respond to |
| | TechNet E-Mail Forum|
| | <[log in to unmask]>; |
| | Please respond to |
| | "Whittaker, Dewey |
| | (AZ75)" |
| | <Dewey.Whittaker@HON|
| | EYWELL.COM> |
| | |
|---------+------------------------------->
>-----------------------------------------------------------------------
---------------------------------------|
|
|
| To: [log in to unmask]@SMTP@Exchange
|
| cc: (bcc: Stephen R Gregory/LABARGE)
|
| Subject: Re: [TN] [OT] RE: [TN] raised vias...I did a "Okie"
cross-section |
>-----------------------------------------------------------------------
---------------------------------------|
I is a half-way measure. Doakie completes the affirmation.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Craig Cullum
Sent: Wednesday, September 14, 2005 5:55 AM
To: [log in to unmask]
Subject: [TN] [OT] RE: [TN] raised vias...I did a "Okie" cross-section
OK, could someone explain to me what "Okie" means please?
TIA
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc. It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message
and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|