TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Brummer Chuck <[log in to unmask]>
Date:
Tue, 13 Sep 2005 08:47:13 -0700
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Brooks,Bill" <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brummer Chuck <[log in to unmask]>
Parts/Attachments:
text/plain (91 lines)
Hi everyone,

Did the boards get sensitized and plated after lamination?  If they didn't
how did you get metal to stick to the resin protruding from the holes?  So
it all seems to depend on the mfg. sequence, it this layer is plated after
lamination then the bumps could be planed down as suggested but they appear
to be far to uniform to be expoxy flowing out of the holes.

Chuck Brummer
AIM/SMS

-----Original Message-----
From: Brooks,Bill [mailto:[log in to unmask]]
Sent: Monday, September 12, 2005 2:54 PM
To: [log in to unmask]
Subject: [TN] raised vias...


Can someone give us a read on what they think cause the raised vias on
Steve's website picture? http://www.stevezeva.homestead.com  page 2.


Bill Brooks - KG6VVP
PCB Design Engineer, C.I.D.+, C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
Datron World Communications, Inc.
_______________________________________
San Diego Chapter of the IPC Designers Council
Communications Officer, Web Manager
http://dcchapters.ipc.org/SanDiego/
http://pcbwizards.com

-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Monday, September 12, 2005 2:28 PM
To: [log in to unmask]
Subject: Re: [DC] Raised vias

Hi Fred and Everybody!

Speaking of "Raised Vias" and "Anthills", I have some anthills on some
Boards that we're building here now.

The anthills aren't from plugging or anything, but are blind via in pad.

I thought that they wouldn't present too much of a problem because I
thought that after printing paste and reflow, everything would level
out...but that wasn't the case.

At locations where I was placing something called a PowerPAK SO8, there was
open solder defects at some of the joints because (I think) of the raised
vias. You can see the PowerPAK part drawing, and the raised vias that I'm
talking about on my web page at: http://www.stevezeva.homestead.com . Go to
"Picture Page 2" and look for "PowerPAK SO8 and Raised Vias".

I don't have a clue why the vias are raised like that...maybe that's a
question for the TechNet.

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2