Hi Kaye,
Sorry
Use IPC 4553 as a reference.
Test the pudding by solderability tests after at least two reflow
processes.
-
Best Regards
Reuven ROKAH
e mail: [log in to unmask]
Kaye Clayo
<kclayo@ To: [log in to unmask]
KEITHLEY.COM> cc:
Sent by: TechNet Subject: [TN] Auditing Immersion Silver processes
<TechNet@
ipc.org>
10/08/2005 18:25
Please respond
to TechNet
E-Mail Forum;
Please respond
to Kaye Clayo
Does anyone have any advice on how to audit pc board
manufacturers immersion silver processes or even
auditing different IAg brands?
Would it be by trial and error? Or is there something
specific to look for?
Thanks in advance.
Kaye Clayo
Sr. P. C. Layout Designer
Keithley Instruments, Inc.
Solon, Ohio
CONFIDENTIALITY NOTE: This message is intended only for the use of the
individual or entity to which it is addressed and may contain information
that is privileged, confidential, and exempt from disclosure under
applicable law. If the reader of this notice is not the intended recipient,
you are hereby notified that any dissemination, distribution or copying of
this communication is strictly prohibited. If you have received this
communication in error, please notify the sender immediately.
_____________________________________________________________________________
Scanned by IBM Email Security Management Services powered by MessageLabs.
For more information please visit http://www.ers.ibm.com
_____________________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to Listserv@
ipc.org: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|