Hi Rich,
Can I assume that:
#1 - the Tg would be over the same range as the CTE.
A: No, The Tg is independent of the range over which the CTE isd measured.
#2 - the Td would be defined at the usual 5% loss point
A: Yes.
Regards,
Werner Engelmaier