Dave,
So far I am going on the assumption that non-RoHS compliant Irradite and
RoHS compliant Irradite both perform equally for the purpose of the
plating. In our case it looks good and reduces pitting and corrosion in
the aluminum. I don't have much (read any) testing budget, so I'm sort
at the mercy of the platers. Hence, the reason I want a way to "hold
them to their word" at least in print.
Phil
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Tuesday, August 23, 2005 4:14 PM
To: [log in to unmask]
Subject: Re: [LF] Specifying RoHS compliant Irradite
Hi Phil! As your "cynical brother in soldering" I have a question - " Do
you know that the RoHS compliant Irradite meets the same functional
requirements as the noncompliant Irradite?" Did you conduct any testing
or
are you using supplier data?
Dave Hillman
Rockwell Collins
[log in to unmask]
Phil Nutting
<PNutting@KAISERS
YSTEMS.COM>
To
Sent by: Leadfree [log in to unmask]
<[log in to unmask]
cc
>
Subject
[LF] Specifying RoHS compliant
08/23/2005 02:46 Irradite
PM
Please respond to
"(Leadfree
Electronics
Assembly Forum)"
<[log in to unmask]
>; Please respond
to
Phil Nutting
<PNutting@KAISERS
YSTEMS.COM>
This may be outside our groups purview, but I'll ask it anyway.
For our aluminum chassis sheet metal we have historically used Yellow
Irradiate. The information I'm getting for making this RoHS compliant
is to make sure the plating vendor used trivalent chromium rather than
hexavalent chromium for either clear or yellow irradiate.
It is also my understanding that there are similar "rules" for zinc
plating.
The real question is, how do I specify this on my assembly drawings and
purchase orders?
Am I going to get a true RoHS compliant plating? I can't be the only
person with this issue!
I'm sure I can go into did the plater have a dedicated RoHS plating
tank, is he telling me he complies but in reality he just lies?
Hey, I'm a cynic.
Phil Nutting
Design for Manufacturing Engineer
Kaiser Systems, Inc.
126 Sohier Road
Beverly, MA 01915
voice: 978-922-9300 x1310
fax: 978-922-8374
e-mail: [log in to unmask] <mailto:[log in to unmask]>
www.kaisersystems.com <http://www.kaisersystems.com/>
------------------------------------------------------------------------
-------Leadfee
Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
------------------------------------------------------------------------
-------
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
(Embedded image moved to file: pic18352.jpg)
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|