Dennis:
We will likely post the SMTA paper/presentation after the conference.
Regarding your other question, shelf life and coplanarity were not part
of our study per se. If coplanarity is important, then you should
select Cu OSP or an immersion coating (Ag, Au or Sn). Cu-OSP may have
the shortest shelf life of these. Our PCB guys favor immersion Ag at
this point.
Cheers,
Bob
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Dennis Bang
Sent: Monday, August 15, 2005 7:17 PM
To: [log in to unmask]
Subject: Re: [LF] Press-fit terminations
Thanks Bob!
Would the update be available online as unless the SMTA conference is
held "down-under" I don't think I can attend :(
But, if you had to choose the best surface finish for press-fit
considering shelf life and coplanarity as influencing parameters, which
one would you choose?
Rgds
Dennis.
-----Original Message-----
From: Hilty, Robert D [mailto:[log in to unmask]]
Sent: Tuesday, 16 August 2005 12:38 AM
To: (Leadfree Electronics Assembly Forum); Dennis Bang
Subject: RE: [LF] Press-fit terminations
Dennis:
We have done some work on press-fit that Dave mentioned. It can be
found on our website under the heading of press-fit terminations at:
http://www.tycoelectronics.com/environment/leadfree/techdata.stm
We will also be presenting an update to this work at the SMTA conference
this fall. We have found that ENIG, OSP, Immersion Ag, Immersion Sn,
Immersion Au and of course HASL (tin lead) work well with tin, tin-lead
and gold plated components. Generally, hole size do not need to be
changed. We have not yet completed our detailed studies on lead free
HASL. The Rohm and Haas work has been encouraging but the info I have
seen has been limited.
Cheers,
Bob Hilty, Tyco Electronics
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Dennis Bang
Sent: Monday, August 01, 2005 4:18 AM
To: [log in to unmask]
Subject: [LF] Press-fit terminations
Hi fellow technetters
From previous discussions on this topic, OSP and Im-Sn are recommended
as the PCB finish.
http://listserv.ipc.org/scripts/wa.exe?A2=ind0402&L=leadfree&P=R328&I=-3
http://listserv.ipc.org/scripts/wa.exe?A2=ind0401&L=leadfree&P=R5429&I=-
3
This info was in 2004. Have there been any updates since for the
preferred PCB finish for Pressfit applications? Has anyone used or
trialed Lead Free HASL for press-fit connectors? Any issues?
Regards
Dennis.
#################################################
***** CONFIDENTIAL *****
We apologise if this message has been sent to you in error. We are
committed to protecting the confidential information of our customers,
our vendors and GPC Electronics. If you have received this message in
error, we would appreciate you removing it from your system and
informing us of the error, so that we may continue to improve our
processes.
Please note that whilst we check our outgoing mail, you should also
check any attachments for viruses and defects before opening them or
sending them on.
Thank you.
#################################################
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d To unsubscribe, send a message to [log in to unmask] with following
text in the BODY (NOT the subject field): SIGNOFF Leadfree To
temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL) Search previous postings at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
#################################################
***** CONFIDENTIAL *****
We apologise if this message has been sent to you in error. We are
committed to protecting the confidential information of our customers,
our vendors and GPC Electronics. If you have received this message in
error, we would appreciate you removing it from your system and
informing us of the error, so that we may continue to improve our
processes.
Please note that whilst we check our outgoing mail, you should also
check any attachments for viruses and defects before opening them or
sending them on.
Thank you.
#################################################
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d To unsubscribe, send a message to [log in to unmask] with following
text in the BODY (NOT the subject field): SIGNOFF Leadfree To
temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL) Search previous postings at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|