Thanks Dave,
I Compared Kester 182 data sheet to J-STD-3 requirements (3.2.2) & it
matches exactly.
Mark
-----Original Message-----
From: [log in to unmask]
[SMTP:[log in to unmask]]
Sent: Wednesday, August 03, 2005 11:15 AM
To: [log in to unmask]; [log in to unmask]
Cc: [log in to unmask]
Subject: Re: [TN] ROL1 flux for solderability testing
Hi Mark! Please keep in mind that the JSTD-002 and JSTD-003 requires
a
specific, defined flux composition recipe and not just any ROL1 flux
per
JSTD-004. Both specification list the exact flux composition
required to
be used. Both the JSTD-002 and JSTD-003 committees have requested
specific
product designation from any/all flux material suppliers to be
listed in
each of the specifications in section 6 of the next revisions.
Dave Hillman
Rockwell Collins
[log in to unmask]
Mark Hargreaves
<[log in to unmask]>
Sent by: TechNet
To
<[log in to unmask]> [log in to unmask]
cc
08/03/2005 09:51
Subject
AM [TN] ROL1 flux for
solderability
testing
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Mark Hargreaves
<[log in to unmask]>
Hi All,
I'm looking for a supplier (in USA) of ROL1 flux (1 gallon or
smaller) for
low volume solder float solderability testing.
Kester 182 looks good (from datasheet) but I can't find a source.
Any suggestions?
Thanks,
Mark Hargreaves
EMDS, Inc
[log in to unmask] <mailto:[log in to unmask]>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at
[log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|