TECHNET Archives

August 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Cheryl Johnson <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Cheryl Johnson <[log in to unmask]>
Date:
Tue, 23 Aug 2005 12:19:24 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (82 lines)
any chance of getting a photo posted?

Sincerely,
-----------------------------------
Cheryl Johnson, C.I.D.+
Manager
ExcelStor US Office, Engineering Services
Email: [log in to unmask]
Tel: (303) 684-7291
Fax: (303) 684-7268
Mobile: (303) 809-5815
-----------------------------------


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of John Parsons
Sent: Tuesday, August 23, 2005 11:08 AM
To: [log in to unmask]
Subject: Re: [TN] solid gold boards


I usually try to abstain from posting non-technical content but - WOW!

John Parsons

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of r Tarzwell
Sent: Tuesday, August 23, 2005 10:50 AM
To: [log in to unmask]
Subject: Re: [TN] solid gold boards

The board is microwave, with 10 micron lines  which are 20 to 25 micron
thick, the only way i could get it to plate was using gold, copper  proved
to be to bumpy   way to many noduels and clumps,  the surface must be
smooth for the frequency, I also had to use very little oxide foot below
to get the  initial thin 2 micron copper to stick to the prepreg,    And
Ni was out because of  to high a frequency,  so the board was not
originaly to be golds just turned out that way,   It has  bga, smt  and
wire bond on it so I needed to be able to advise the assemblers how to try
and solder it, Im not down to the 10 micron yet ( 20 now) but will be
investigating a beter laser.   and to boot the micro vias are only 30
microns.  a fun but  tough board   good thing its only 1 inch square.
bob

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2