Werner,
As usual you are correct. You also have to know the solder composition
that these materials are dissolving into. The values I quoted are for
dissolution into SnPb solder (eutectic or near eutectic 60/40) at a
temperature of approximately 210C.
Regards,
George
George M. Wenger, Andrew Corporation
Reliability / FMA Engineer
Base Station & Subsystems Group
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 [log in to unmask]
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Monday, August 22, 2005 11:15 PM
To: [log in to unmask]; Wenger, George M.
Subject: Re: [TN] max thickness electroplated gold
Hi George,
Now, of course, you need to add for which temperature these values were
measured, and add that they will vary greatly with temperature.
Werner
------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
[mf2]
|
|
|