Karen
Are you sure it is ON the conformal coating?
I assume you apply the conformal coating after the push fit connectors?
Do you clean the assembly? If so, by what material and method?
Under what conditions do these growths appear?
--
Regards Graham Naisbitt
[log in to unmask] [log in to unmask]
Golf Quote of the week: You can talk to a fade but a hook won't listen.
CONCOAT SYSTEMS LIMITED
Unit B2, Armstrong Mall
Southwood Business Park
Farnborough GU14 0NR
Phone: +44 (0)12 5252 1500
Fax: +44 (0)12 5252 1112
CONCOAT - Engineering Reliability in Electronics
CONCOAT SYSTEMS - Measuring Reliability in Electronics
A British Manufacturer
www.concoat.co.uk & www.concoatsystems.com
Cell: 079 6858 2121
On 2/8/05 12:50, "Karen Walters Ebner" <[log in to unmask]> wrote:
> We recently moved from soldered connectors to press fit connectors. Since
> this time randomly we observe on boards between the pin on top of the
> conformal coating a white material growth between the connector pins. We
> are going to investigate the what type of contamination may be on the
> board but if you were going to list most probable causes and corrective
> actions what would they be?
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|