Thanks all for your help.
We have decided to build a small humidity and temperature storage room for all MSD's and circuit cards, as well as a McDry cabinet for incoming inspection storage. Also we will start enforcing our internal requirements to our fab houses for proper handling, storage, and packaging. On top of that our internal procedures governing handling, storage, and packaging of MSD's is under review for update once I have received IPC docs. IPC-J-STD-020C, J-STD-033A, and the soon to be released J-STD-030.
Again, thanks for all your help.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Creswick, Steven
Sent: Tuesday, August 30, 2005 8:24 AM
To: [log in to unmask]
Subject: Re: [TN] ENIG/ Immersion Gold Plating and Pre-baking &
Solderability
Richard,
Is it an approved/acceptable process to place the PWB's into a vacuum chamber at room temp?
I would not hazard a guess as to how great of a vacuum for what duration, however. Just curious if it is done in the surface mount industry.
Nothing gets any more simple than a dessicantor box though!
Steve Creswick - Gentex Corp
-----Original Message-----
From: Stadem, Richard [mailto:[log in to unmask]]
Sent: Tuesday, August 30, 2005 9:05 AM
To: [log in to unmask]
Subject: Re: [TN] ENIG/ Immersion Gold Plating and Pre-baking &
Solderability
Baking of ENIG plated boards may be a requirement in order to drive out
moisture even though it can exacerbate a nickel oxide formation that is
already started. But there are other options for moisture removal,
including lower bake temperatures at longer times. You could even lease
a precision scale and see at what length of time is required for simply
putting the PWB into a drybox (a dessicator box such as McDry, not a
nitrogen box) and allowing it to dry at room temperature for a period
long enough to reduce the moisture content by 90% or more. J-STD-030
does state that the bake times and temperatures they list for components
and pwbs are guidelines. If you can prove your bake process or
dessication process is removing the moisture, then you are qualifying a
lower temp and longer time. You will need to use a number of pwbs in
order to do this, as there is some variation in weights caused by resin
content, etc. But you should be able to show a reduction in the average
of weights (mean weight).
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Schaefer
Sent: Friday, August 26, 2005 10:10 AM
To: [log in to unmask]
Subject: [TN] ENIG/ Immersion Gold Plating and Pre-baking &
Solderability
Does baking these types of plating affect solderability? If so what
factors play a part (i.e. baking temperature, plating thickness, baking
time, etc...). I know that if baked it can cause the Nickel Oxide layer
to become less solderable if the plating process is Poor (thanks Richard
S.). Is there is a factual study that proves that baking any type of
gold plated boards in any way shape or form reduces the solderability
and/ or reliablity of the joints/ product? I am trying to gather data to
prove to management that baking is a bad decision with this type of
plating and should never be performed. Also if a Gold Plated board of
any type is suspect for high level moisture content - how do you remove
the moisture "IF" baking is not acceptable?
Chris Schaefer
Suntron Corporation
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|