I don't have any curves but consider CTE of BeO to be 7.2-7.6 ppm in the range of 25-300°C [based on data from 4 sources], whereas I only have one data point for GaAs in the 25-300°C range and that is 6.5 ppm
Since the AuSn eutectic is right at 280°C [or maybe 282°C as I have seen in some places], you should be placing the device under compression as the substrate cools down. This is better than the alternative!
Pretty funky aspect ratio on the chip!
Like to know if anyone else has better values so as to update my database...
Steve Creswick - Gentex Corporation
-----Original Message-----
From: Sundog [mailto:[log in to unmask]]
Sent: Monday, August 29, 2005 1:34 PM
To: [log in to unmask]
Subject: Spam: [TN] GaAs and BeO Coefficient of Therma Expansion curve
Dear all,
Does anyone has a GaAs CTE curve (vs. temperature). I am trying to solder a
10mmx1mmx0.14mm GaAs die to a BeO substrate with AuSn solder. I am not
quite sure if there CTE is matched well enough.
Thanks
Sundog
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|