TECHNET Archives

August 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Date:
Thu, 25 Aug 2005 15:14:21 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Eddie Rocha <[log in to unmask]>
Subject:
From:
Eddie Rocha <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (69 lines)
If the blistering originates from the vias and they are
covered with soldermask, then I would suspect the
soldermask in the hole isn't fully cured. This could lead
to blistering.

Thank you,
Eddie Rocha
South Bay Circuits


Hi Technos,

wanted to start a pilot run, but the first PCB that we
soldered ended up full of blisters when it came out of the
oven. It is a 6 layers, full ground and power planes, about
6"x7", not a high density one, pretty light stuff on it,
the toughest part is a transformer which needs a little
more heating. The profile peaks at 250C on the PCB itself
and the PCB is made out of FR4, Tg 170.

I said to myself that it must be humidity, so I baked 1
board, 8H @ 125C, and passed it through the reflow again.
Same blistering, almost to the same extent. Then I took a
totally different PCB that was hanging around on my desk
for about 3 months, reflowed it at 250C and got just a tiny
blister, probably due to humidity this time.

The questions I have are:

is 250C too much for a properly manufactured PCB?

If it's not the humidity what else could it be?

Any other test that I could do to get a better idea of the
root cause?

Thanks,
Ioan



---------------------------------------------------
Technet Mail List provided as a service by IPC using
LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with
following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send
e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at
[log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2