Sounds like you have something set up for maybe a microwave application???
Gold ribbon bonding, gold wire bonding, or TAB bonding maybe.
..... I could certainly find a use for any extras which you might have :-)
Steve
-----Original Message-----
From: r Tarzwell [mailto:[log in to unmask]]
Sent: Tuesday, August 23, 2005 9:06 AM
To: [log in to unmask]
Subject: [TN] solid gold boards
hi guys and girls, i have a solid gold board , the tracks are soild plated
gold about 25 microns thick , no ni, over 2 microns of copper (outer
space reasons) and i was wondering how to solder the components , would
the soild gold traces cause brittle joints, or would the large gold ratio
allow a good soilder joint with lead free solder or any type of solder. I
have no experiance with soild gold at all and was hoping some one out
there would has a guess. PS the traces are only 10 microns wide in areas
which is an other problem
robert Tarzwell
director of technology
Sierra Proto express.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|