TECHNET Archives

August 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 18 Aug 2005 09:26:02 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (68 lines)
 

        From an article:

Flux-induced corrosion (Copper Mirror Test)
A measure of the chemical corrosivity of a flux, the copper mirror test is referenced in a number of specifications (such as IPC-TM-650 Method 2.3.32), and is in common use as an indicator of the level of soluble ionic and aggressive activators in a flux. The test assesses the corrosion by cold flux (23°C) in a humid environment (50% RH) of a very thin film of copper on a glass slide: if there is significant corrosion, the film becomes transparent.

For liquid fluxes, the test involves placing two drops of a 35% solution of the flux on a 'copper mirror'. This is a glass microscope slide on which has been deposited approximately 30-50nm of copper, defined as a Cu thickness which allows the transmission 10±5% of normally incident 500nm wavelength light. Typically, a flux made of pure water-white gum rosin and isopropanol acts as a control, and a drop of it is also placed on the mirror. The mirror is then placed in a controlled environment of 23±2ºC and 50±5% relative humidity for 24 hours, rinsed in isopropanol and examined for any spots or areas where the copper has been removed by the flux.

The test has several drawbacks which have led critics to question its relevance.

The test indicates the potential corrosivity of the raw or unheated flux, which is not always indicative of the corrosivity of partially-heated flux (such as flux present on the component side of an assembly during wave soldering) or of fully heated flux (such as flux on the wiring side of a board) 
The results can be difficult to interpret, being somewhat subjective and with no middle ground between pass or fail. 
However, the test is quick and easy to perform, and its results correlate well with those of the more lengthy and involved surface insulation resistance test. It is widely accepted and is especially useful as a pre-screening test when testing a new formulation or as a routine incoming materials check.

In some versions of this test, it is applied to solder paste by first extracting any ionic species by boiling a sample of paste in solvent (propan-2-ol) and then concentrating the extract to approximately 35% solids by weight. It has been suggested, correctly, that this procedure is unfairly weighted against pastes with a low-solids flux content, so IPC-TM-650 Method 2.3.32 applies solder paste direct to the mirror.
        ramon




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak
Sent: Wednesday, August 17, 2005 3:41 PM
To: [log in to unmask]
Subject: Re: [TN] Copper Mirror test for water-based fluxes

For those of us who only recently realized that something had to happen to a PCB before it was installed..(Assembly?  What's that?)... be so kind as to tell us more about this test, and what it is supposed to tell you... and how to read it....

Any help is appreciated...(and needed)

Rudy Sedlak
RD Chemical Company

Bev Christian <[log in to unmask]> wrote:
It is such a long time that I have done one of these, that I don't remember what we did to evaporate the water! The alcohol based ones are easy, but the water ones?! Do you just let them set at room temperature or do you give them a little heat or what?
Bev
RIM




---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

__________________________________________________
Do You Yahoo!?
Tired of spam?  Yahoo! Mail has the best spam protection around

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
http://mail.yahoo.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2