What was the difference of soldering versus dipping?
One does not solder to the gold, it is quickly absorbed into the solder,
and then you form the IMF with the nickel underneath. If they did not
solder with the gold on them, why would they solder with the gold
removed?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee parker
Sent: Thursday, August 18, 2005 7:54 AM
To: [log in to unmask]
Subject: Re: [TN] HASL over nickel
Richard
There could be many reasons. several years ago I was working with an OEM
who had ENIG boards and on New Years Eve discovered they would not
solder. We removed the gold by dipping the boards into a large solder
pot and then dipped them into a second solder pot to insure a solderable
surface. This removed the gold and left a highly solderable coating of
solder over the nickel. The boards were then assembled (on New Years
Day) which allowed the systems to be shipped on time the day after.
Best regards
Lee
----- Original Message -----
From: Stadem, Richard<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Thursday, August 18, 2005 7:53 AM
Subject: Re: [TN] HASL over nickel
Why ever would you want to do this? Why not just solder to the ENIG?
Is
there some requirement that precludes soldering to the ENIG?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tom Moore
Sent: Wednesday, August 17, 2005 2:38 PM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: [TN] HASL over nickel
Our PC board supplier inadvertently supplied us with boards composed
of
gold over nickel rather than the specified HASL finish. While we kept
some of the boards to keep our production line running, we sent the
rest
back to have the gold stripped off and run through the HASl process.
Now
our supplier is telling us that they will not be able to remove the
nickel that has bonded to the copper pads. I'm going to have the
supplier guarantee the board life in blood, but I would feel more
confident in having confirmation by this group's expertise. Thanks for
your help.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to
[log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or
(re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET
Technet Digest Search the
archives of previous posts at:
http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please
visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/cont
entpage.asp?Pageid=4.3.16> for
additional information, or contact Keach Sasamori at
[log in to unmask]<mailto:[log in to unmask]> or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to
[log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/cont
entpage.asp?Pageid=4.3.16> for additional information, or contact Keach
Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|