Perhaps the same flux should be used on a different board that
has no solder mask or different solder mask. It would determine whether
the solder mask is reacting or not.
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard
Sent: Tuesday, August 16, 2005 8:36 AM
To: [log in to unmask]
Subject: Re: [TN] White residues at wave soldering
I agree with Brian's assessment. It appears in the pictures that the
white mongue does not appear on the solder joints, only on the solder
mask in this case. Therefore I am led to believe that it is some type of
a reaction with the solder mask.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Tuesday, August 16, 2005 2:43 AM
To: [log in to unmask]
Subject: Re: [TN] White residues at wave soldering
Impossible to say without a full rundown of all your materials and
processes. However, if this happens with only one flux, I would suggest
you start looking at an incompatibility between some component in the
flux and the solder mask. What you ***may*** be seeing is the surface of
the mask being very slightly attacked, exposing fillers which would
normally be invisible.
Brian
Peter Lee wrote:
> Technet,
>
> I have a question on white residues formation at wave soldering. We
> have recently run experiments to test the performance of various
> halide-free water soluble fluxes (ORH0 under JSTD-004). The flux was
> applied through a spray fluxer and all PCAs were immediately washed
> after wave soldering in in-line cleaner, with DI water only.
>
> Surprisingly, we've identified several PCAs built with flux A from one
> vendor exhibiting white residues at various T/H leads on the boards.
> See images below.
>
> http://members.shaw.ca/ppwlee1/Images/White_residues1.JPG
> http://members.shaw.ca/ppwlee1/Images/White_residues2.JPG
>
> What could be the cause and forming mechanism of the residues? What
> causes it to become (sometimes) insoluble in water? In general what
> approach can be taken to minimize or prevent formation of white
residues?
>
>
> Rgds,
> Peter
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
--
______________________________________________
Please note new e-mail address [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|