And the tin residue presumeably "poisons" the subsequent nickel deposition
and leads to skip plating on the enig - right?
Yes a lot of experience on detecting the condition but I can tell you that
if the drilled hole is 10 mils and the board thickness is over 90 mils that
you are approaching the limits.
I designed a test vehicle which I called the "bernoulli bus" which will tell
you where the edge of your process capability is.
If you would like to call me I can tell you how to do that - mobile is
better.
Kind regards,
John Burke.
------------------------------------
Avanex
John Burke
Senior Manager RoHS Compliance
[log in to unmask]
40919 Encyclopedia Circle
Fremont
CA 94538
tel: 510 897 4250
fax: 510 979 0189
mobile: 510 676 6312
------------------------------------
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Greg Triggs
Sent: Wednesday, August 10, 2005 12:48 PM
To: [log in to unmask]
Subject: [TN] Tin Strip
Hello
With the advent of hign aspect ratio holes. Has any out there
come up with new ways to get stripper solution movement thru the holes for
good stripping? We are using a Chemcut fixed manifold conveyorized unit.
Surface looks good, but we sometimes leave tin in the holes. Have used fluid
heads as the last spray, but this was a mess.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Thanks in advance.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|