I would use the recommended operational guidelines of the chemical
supplier to start and then validate any differences noted with the
supplier. The rinse cycle is of particular importance to reduce the
yellowing after TC.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice: 802.257.4571.21 Fax: 802.257.0011
http://www.vtcircuits.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kaye Clayo
Sent: Wednesday, August 10, 2005 11:26 AM
To: [log in to unmask]
Subject: [TN] Auditing Immersion Silver processes
Does anyone have any advice on how to audit pc board
manufacturers immersion silver processes or even
auditing different IAg brands?
Would it be by trial and error? Or is there something
specific to look for?
Thanks in advance.
Kaye Clayo
Sr. P. C. Layout Designer
Keithley Instruments, Inc.
Solon, Ohio
CONFIDENTIALITY NOTE: This message is intended only for the use of the
individual or entity to which it is addressed and may contain
information that is privileged, confidential, and exempt from disclosure
under applicable law. If the reader of this notice is not the intended
recipient, you are hereby notified that any dissemination, distribution
or copying of this communication is strictly prohibited. If you have
received this communication in error, please notify the sender
immediately.
________________________________________________________________________
_____
Scanned by IBM Email Security Management Services powered by
MessageLabs. For more information please visit http://www.ers.ibm.com
________________________________________________________________________
_____
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|