Aluminum oxide is the principal phase most "Ceramic" packages, excluding
most LTCC packages, IBM's low CTE ceramic, and the Hi-CTE ceramic packages
that are available. Calling the PGA body an alumina ceramic or aluminum
oxide ceramic is perfectly correct. It is understood that such a ceramic is
about 90-92 wt % alumina.
Best regards,
Leo
Leo M. Higgins III, Ph.D.
Director of Applications Engineering
ASAT, Inc.
3755 Capital of Texas Highway, Suite 100
Austin, Texas 78704
ph 512-383-4593
fx 512-383-1590
[log in to unmask]
www.asat.com
The information contained in this electronic message is CUSTOMER/SUPPLIER
PRIVILEGED AND CONFIDENTIAL INFORMATION intended only for the use of the
individual or entity named above. If the reader of this message is not the
intended recipient, you are hereby notified that any dissemination,
distribution and copying of this communication is strictly prohibited. If
you have received this communication in error, please immediately notify the
sender by electronic mail. Thank you.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Stadem, Richard
Sent: Monday, July 11, 2005 4:21 PM
To: [log in to unmask]
Subject: Re: [TN] Moisture Sensitive Components (again)...
Steve,
Many out there are experiencing the same thing.
But not for components such as aluminum oxide (not really ceramic) like
what I think your picture shows.
They may have lead-free finish on the pins, but that does not make them
a candidate for special handling to prevent moisture-related
expansion......usually. It is possible that there is a chance of damage
within the encapsulant. Really hard to tell without consulting the
vendor.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stephen Gregory
Sent: Monday, July 11, 2005 4:00 PM
To: [log in to unmask]
Subject: [TN] Moisture Sensitive Components (again)...
Hi all ya'll!!
Haven't heard anything from my big mouth in quite a while have ya'?
Well, I just got back from two glorious weeks of vacation in beautiful
(but rainy) North Carolina...that's why I've been so quiet.
Anyways, it's about Moisture Sensitive components. You may recall my
posts from a while back about us trying to get our stockroom people more
in tune with MS components and proper handling, and they've been doing a
great job. They come to me with a lot of questions and I actually like
that. Shows me that they're trying to make sure they get it right.
Well today one them came to me today with some parts that were packaged
and labeled MSL 3, but they were ceramic Pin-Grid-Arrays?!?
You can how they were packaged and labeled at:
http://www.stevezeva.homestead.com click on Picture Page 2 and look at
Ceramic PGA Packaging to see how they came to us.
I've always thought that ceramic parts were not subject to moisture
related concerns, am I wrong once again?
It's a Cypress part, PN # 5962-9759802QXC (Military part). I called
Cypress, to verify if it was a MS component or not, and got their
outsourced technical support line (I think from India), and I was told I
had to "submit a case"
email
to get my question answered.
I think somebody suggested last time when I posted about this, that
distributors are putting MSL labels on everything just to be safe,
whether a component is MS or not....are any of you experiencing this?
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential
to LaBarge, Inc. It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message
and kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|