Steve...
That isn't normal.....
It looks like the epoxy lid seal ring has been over heated in the
corners...
Paul
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stephen Gregory
Sent: Wednesday, July 27, 2005 9:35 AM
To: [log in to unmask]
Subject: [TN] Strange Looking BGA Heatsink Gap...
Hi Everyone!
We just finished building 8-assemblies that used a 780-ball Altera
Stratix
BGA on them. These BGA's have a pretty decent sized copper heatsink
in the top.
Everything went pretty good. But then I noticed something with the BGA
heatsink after we got them all built. In the corners, there seems to be
some
sort of gap beneath the heatsink and the top of the part that I didn't
notice
before. Go to: http://www.stevezeva.homestead.com then click on Picture
Page 2, then look for "Heatsink Gap".
All the BGA's show this in all 4-corners. I don't have any more of these
BGA's
around that haven't been through reflow, so I can't do a before and
after
reflow
comparison. The Altera package drawing doesn't show this gap either.
I'm thinking (hoping) that the parts are made like this, to somehow keep
the
whole part from warping during reflow because of a CTE mismatch between
the
substrate and the heatsink...it just looks strange though.
Anybody else out there familiar with these devices that can tell me this
is
normal?
(Please tell me this is normal!!)
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc. It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message
and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|