Hi Ted
The real story on the web is:
Cadmium in cables exceeded 0.01% limit by 3-20x
- Sony forced to replace and destroy non-compliant cables
before PS1 shipments could continue
- No recall of existing units, and no replacement in other
countries where cadmium levels did not exceed local
regulations
Best regards
Mario
-----Message d'origine-----
De : Ted Tontis [mailto:[log in to unmask]]
Envoyé : 27 juillet, 2005 11:10
À : TechNet E-Mail Forum; Dion, Mario
Objet : RE: [TN] RoHs compliant toner (ink) for laser printer ?
It cost Sony millions due to a label, they had to recall a ton of play
stations from the Netherlands.
Ted
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dion, Mario
Sent: Wednesday, July 27, 2005 9:49 AM
To: [log in to unmask]
Subject: [TN] RoHs compliant toner (ink) for laser printer ?
Bonjour TechNeters,
Here is a question about RoHs. One customer is requesting that we comply
with RoHs and mentionned that there could be a concern with laser ink
used
on the product labels we affix on finish products.
I have made some verifications with HP but have not get any firm answer
as
of yet.
Do you ever heard about a problem for the ink to comply with RoHs
requirements ?
Thanks for your collaboration
Mario Dion, A.Sc.T.
Sr Project Manager
Solectron EMS Canada Inc.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|