TECHNET Archives

July 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Art Glass <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Art Glass <[log in to unmask]>
Date:
Wed, 27 Jul 2005 08:11:54 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (24 lines)
At a previous job, we did SMT followed by chip-and-wire on a regular basis
for many years, through several product life cycle iterations. The best
solution to keeping the wirebond pads clean was a peel-off temporary solder
mask. Tech Form, which is now a division of Kester, has a whole series of
temporary masks. Selection of specific product depends on the cleaning
processes you use after SMT. Some can be stencil printed down to just a few
mils thick, so as not to mess up stencil printing your solder paste. Oven
cures in a half hour or less, peels off with tweezers right before die
bonding.
As for gold intermetallics with 40 microinches of gold, we had a
metallurgist work with us and established that as long as time above
liquidus was sufficient, the IMCs were distributed (dissolved?) enough into
the joint so as not to be a risk.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2