I see this in many designs.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice: 802.257.4571.21 Fax: 802.257.0011
http://www.vtcircuits.com
-----Original Message-----
From: Stephen Gregory [mailto:[log in to unmask]]
Sent: Friday, July 22, 2005 3:33 PM
To: [log in to unmask]
Subject: Re: [TN] layman's definition of theiving
Or, it can apply to theiving pads which are extra pads in
a SOIC footprint for a part that is going to be wave soldered.
The extra pads are placed besides the last pads of the footprint
that will be going over the wave. Supposedly, this will prevent
solder bridges.
I haven't seen them used enough to tell you whether or not that
works...
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
|---------+---------------------------->
| | Franklin Asbell |
| | <[log in to unmask]
| | NET> |
| | Sent by: TechNet |
| | <[log in to unmask]>|
| | |
| | |
| | 07/22/2005 02:13 |
| | PM |
| | Please respond to|
| | TechNet E-Mail |
| | Forum |
| | <[log in to unmask]>|
| | ; Please respond |
| | to Franklin |
| | Asbell |
| | <[log in to unmask]
| | NET> |
| | |
|---------+---------------------------->
>-----------------------------------------------------------------------
---------------------------------------|
|
|
| To: [log in to unmask]@SMTP@Exchange
|
| cc: (bcc: Stephen R Gregory/LABARGE)
|
| Subject: Re: [TN] layman's definition of theiving
|
>-----------------------------------------------------------------------
---------------------------------------|
Thieving is nothing more than added copper (usually in a specific
pattern,
crosshatch, dots, etc) in non-functional areas of the board, applied for
the
purpose of providing a more uniform surface area during electroplating.
Common uses are where there are long isolated traces leaving areas of
more
dense copper features.
Was that laymen?
Franklin
----- Original Message -----
From: "Phil Nutting" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, July 22, 2005 1:34 PM
Subject: [TN] layman's definition of theiving
Ok, I have to admit my lack of knowledge.
Can someone point me to a the Cliff's Notes version of Theiving on PC
boards?
Thanks in advance.
Phil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc. It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message
and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|