TECHNET Archives

July 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Dehoyos, Ramon" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Dehoyos, Ramon
Date:
Tue, 19 Jul 2005 08:59:22 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (120 lines)
        Hi Richard:
                        I am very interested in your findings, will you
please send me your evaluation results?
        Regards,
        Ramon 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard
Sent: Monday, July 18, 2005 4:04 PM
To: [log in to unmask]
Subject: Re: [TN] BGA voids

Voids can be caused by a number of things, but the most common cause is
the moisture content of the solder paste, and its condition.
That being said, a certain paste that has been known to be the mainstay
for many years currently is the worst one today as far as voiding. A
different paste manufacturer made an excellent paste that was formulated
to prevent voiding.
I recently performed a paste evaluation of standard 63/37, a leadfree
water soluble, and a leadfree no clean paste. There were 27 different
tests, with 5 vendors. On the standard 63/37, the paste formulated to
prevent voiding had ZERO voids in 1330 BGA joints, multiplied by 15
samples. The previous paste vendor had voids in every single BGA joint.
All variables were strictly controlled, and I did not know which sample
was being tested (they were numbered by someone else to prevent any
bias).
While I do not want to give out vendor names on the forum, I would be
glad to share this info with anyone offline.
The application engineer who told you not to worry about voids should be
taken outside and shot. While some data exists that says voids are OK if
they are small enough, you should certainly strive for an alloy that
provides you with an excellent grain structure free of voiding, with
evidence of good IMF at the pad/ball interface. Sorry, pal, but you
cannot determine this with an X-ray machine. It can only be done with a
good microsectional analysis.
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stephen Gregory
Sent: Monday, July 18, 2005 1:07 PM
To: [log in to unmask]
Subject: [TN] BGA voids

Good Day Technetters!

I have a question about BGA voids. We are bidding on some work and it
looks like they have taken statements that are in the IPC-7095, and
placed them as notes on their drawing.

One of the notes has to do with a limit on the percentage of balls on a
BGA device that are allowed to have voids. For example; "Less than 5% of
the balls can have voids, and the percentage of the void area must meet
class
3 requirements."

I can understand the void area being critical, but the percentage of the
number of balls that are allowed to exhibit them?

The reason that I'm asking, is that I was told last week by a
application engineer from a x-ray machine company (who shall remain
nameless), that seeing voids is normal. Just as long as they aren't too
big, or being concentrated at either the pad/ball interface, or the
ball/device interface.
He said you should worry if you don't see any voids on BGA's with
eutectic balls.

Just curious as to what you all think about this?

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential
to LaBarge, Inc.  It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message
and kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2