TECHNET Archives

July 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 12 Jul 2005 19:04:40 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=iso-8859-1
Subject:
MIME-Version:
1.0
Content-transfer-encoding:
quoted-printable
From:
Stephen Gregory <[log in to unmask]>
Parts/Attachments:
text/plain (95 lines)
Here's the latest email exchanges:
                                                                            
                                                                            
                                                                            
                                                                            
                                                                            
 Hello Stephen,                                                             
                                                                            
 Thank you for using the Cypress On-Line ConnectionCenter?.                 
                                                                            
 Q: What do you mean by; "The part is pruned"...I don't understand. I want  
 to know what the gold thickness is on the leads of the part.               
                                                                            
 A: Unfortunately, the 5962-9759802QXC had a Last-Time-Buy of 5th May 2004  
 and there is no pin-for-pin replacement part available.                    
 Could you please let us know if you still require the gold thickness on    
 the leads of the part.                                                     
                                                                            
 (Now the time frame of "Pruning" the part has shifted a year from the last 
 email....still no gold thickness reference which I asked                   
 about in the first place.)                                                 
                                                                            
                                                                            

My response:
                                                                            
                                                                            
                                                                            
                                                                            
                                                                            
 Yes, I still do want to know the thickness of the gold plating on the      
 leads of the part. We have the part in our possesion,                      
 and are going to use it in a printed circuit assembly...I know the part is 
 no longer available. Our customer did a buy of the                         
 part before it was obsoleted.                                              
                                                                            
 ************************************************************************** 
 ******************************************************                     
                                                                            


So, after two-days, I still don't know what the gold lead plating thickness
is. I still haven't received a reply
on the moisture sensitive rating of the component...ain't this s%#@t
FUN?!?

We have a schedule to meet for our customers, and we need information from
OEM component manufacturers
in a timely manner to determine if things comply with accepted industry
standards.

It's almost like they don't care...they throw things over the wall...and
this episode is a perfect example.

When I have to go through drills like this, I want to pull my hair out!!!!!

I know Microsoft, now Cypress, and other large companies have started to
outsource technical support overseas.

In speaking with the individuals, they are really trying to do the best job
that they can. They are very personable,
and very eager to try and be as helpful as they can...but here you go.

You see what kind of difficulties I have come across in trying to find an
answer to what I thought was a simple, and
basic question. I still haven't gotten an answer.

Pretty sad customer support if you ask me...


Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2