Phil,
I have heard a rumor, never substantiated for me anyway, that the lumber
industry got an exemption, so IF that is true and that is where you are
shipping, you can be as happy as a pig in...
Otherwise you have a problem. The 0.1% applies to the weight of the
lead finish, not the product weight, not the circuit pack weight, not
even the component weight.
You have a problem.
Regrets,
Bev
RIM
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: July 6, 2005 2:08 PM
To: [log in to unmask]
Subject: Re: [LF] definition of Homogeneous
Hmmmn? So in our example we have some power modules built for the heavy
equipment industry in which the manufacturer's are stating they have no
intention of making the parts RoHS compliant. There is no alternate for
this part form any other manufacturer.
Does this mean I can't ship my finished product that contains one or
more of these modules?
Does the 0.1% exclusion count to allow me to ship these finished
products?
My design engineer is asking me what to do. My best answer so far is,
"I dunno!"
Phil
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Wednesday, July 06, 2005 1:45 PM
To: [log in to unmask]
Subject: Re: [LF] definition of Homogeneous
Phil,
A homogeneous material is either:
a compound
an element or
a mixture that is the same throughout.
Examples of the three are:
Sodium chloride - Table salt (if you exclude the added potassium iodide
:) )
Aluminium
A brick
The REALLY stupid part in all this is the EU saying that the finish on a
leadframe is mechanically separable from the lead itself. As a chemist,
I might be able to do it chemically, but make one awful mess in the
process.
Does that help?
Bev
RIM
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: July 6, 2005 1:34 PM
To: [log in to unmask]
Subject: [LF] definition of Homogeneous
Good Afternoon,
It may have been discussed, but can some one point me at a layman's
definition of homogeneous as it pertains to lead-free. All the
definitions I have seen make my eyes roll into my head and leave me
babbling in the corner. I need to be able to explain this in plain
English to my engineering force.
Thanks in advance,
Phil Nutting
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|