Good morning Mary "J",
In response to your question we could go to J-STD-001, 9.2.5.1. This
refers you to table 9-1, however to be more clearly understood you can
look at the cut away in fig.3. Through the barrel of the board the
circumferential wetting has to be 270 deg. voids or pin holes would cause
this to be considered "minimum acceptable condition class 1, 2. The 270
deg pertains to the solder source side of the lead and barrel, if you have
a desk reference manual DRM-40, you will be able to see more quickly to
make your decision.
IPC-A-610D, 7.5.5.4, fig.7-118 gives a very clear example and so will
7.5.5.2 show examples of the primary side acceptable standards. It sounds
like a possibility of the lead size and maybe clinch configuration of the
component.
I'm sure you will be getting quite a few responses from the great Guru's,
They have far more knowledge of these incidents. Hope this helps in so
small way.
Have a blessed day.
P. Lance Mayes CIT
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Mfg. Trainer
|
|
|