TECHNET Archives

July 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 13 Jul 2005 10:31:17 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Genny Gibbard <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Genny Gibbard <[log in to unmask]>
Parts/Attachments:
text/plain (85 lines)
Sounds like the exact same type of response I am getting from other semiconductor mfrs.
This does not seem to be isolated to Cypress, unfortunately.
However, the co I was dealing with last week, (and am still waiting for a final response...ahemTI..ahem) sent out an automated customer satisfaction survey for me to fill out, based on my experience with the tech support.
I gleefully filled it out...  It felt good to get some of that out of my system...  but the person handling my call might not feel as good about it.
The thing that bugged me the most was that most of the response was info reposted from the website.  They assumed I hadn't bothered to look there first, I guess.  I searched the website thoroughly before I tried the help.  I only tried it once I was sure my question wasn't being answered anywhere else.
And that is just one of the stories I could tell right now.  My requests are all about researching parts for RoHS

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Stephen Gregory
Sent: 13-Jul-05 6:43 AM
To: [log in to unmask]
Subject: [TN] Continuing Cypress part saga...you're not going to believe
this


Mornin' once again!

Opened my email this morning to find another response from Cypress.
YAY! I thought to myself, I'm finally getting an answer!

I opened the email which links you to the Cypress web page, then to your
case number. I opened my case, and this is what I found:






 Thank you for using the Cypress On-Line ConnectionCenter.
 We are from Quality System & Customer Support Group. Your request is
 important to us.
 We'll start working on this case and give you complete response on or
 before 7/27/05.

 Best Regards,
 Rose Sandoval
 Quality Systems & Customer Support
 Cypress Manufacturing Limited, Philippines




Can you believe this!?? I should have just went ahead and tinned the part
in
the first place without bothering to ask the company that made the part how
thick the gold is that they plated the part with.

I never would have thought that it would take over two weeks to answer such
a simple question as that. SHEESH!

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2