TECHNET Archives

July 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Edwin Louis <[log in to unmask]>
Date:
Fri, 8 Jul 2005 12:41:18 -0400
MIME-Version:
1.0
X-To:
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (21 lines)
We have a 256 leaded BGA with pads on the perimeter in which the solder
flows over the stringer solder mask barrier and fills up the attached via
hole and pad and causes a short circuit. The component pad size is 0.6mm
dia., the ball dia. Is 0.75mm, the pwb pads are nsmd and 0.71mm dia. This
part weighs 8 grams. Another plastic BGA on the board weighing 2 grams has a
0.6-0.9mm ball and 0.584mm pads. The PWB pads are the same as the other part
but the 357 leads are in a square center pattern. The 256 leaded part ends
up 0.46mm off the board while the 357 leaded part ends up 0.74mm off the
board. Can someone give an idea why this is happening?


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2