Laser/photocopier toner is a powder comprising essentially a wax and a
finely ground pigment. I would be VERY surprised if black toner
contained anything reprehensible, as the pigment is essentially carbon
black, which is produced industrially by the condensation of sublimed
carbon produced by burning a hydrocarbon with insufficient oxygen to
ensure complete combustion (e.g., the black deposit on the chimney of an
oil lamp with too much wick exposed). Coloured toners may be different,
but I doubt whether pigments like cadmium yellow or litharge would be
used, as grinding them would be a very hazardous process.
I would also be very surprised if the wax could contain any
RoHS-designated substances, either.
But have you thought about the label itself or its adhesive? :-) :-)
Brian
Dion, Mario wrote:
> Bonjour TechNeters,
>
> Here is a question about RoHs. One customer is requesting that we comply
> with RoHs and mentionned that there could be a concern with laser ink used
> on the product labels we affix on finish products.
>
> I have made some verifications with HP but have not get any firm answer as
> of yet.
>
> Do you ever heard about a problem for the ink to comply with RoHs
> requirements ?
>
> Thanks for your collaboration
>
>
> Mario Dion, A.Sc.T.
> Sr Project Manager
> Solectron EMS Canada Inc.
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
--
______________________________________________
Please note new e-mail address [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|